Khongor
MongoliaUnknown
Overview
Chip samples: 1.84% Au, 0.43 g/t Au, >300 ppm Mo. Intersections: 70.3 m at 0.67% Cu, 0.16 g/t Au; 91.7 m at 0.3% Cu, 0.08g/t Au; 50 m at 1% Cu, 0.3 g/t Au.
Geological Context
Host Rock: breccia, feldspar porphyry, hornfels ()
Resources & Operations
Data Provenance
Source: USGS MRDS